Thank you for the insights!

View Article


Reply To: Tolerances before or after anodizing?

Ciao Nick,for my experience I can only tell you: it depends.We must admit that normally the treatment must be performed on finished product after all the working and therefore on precise...

View Article


Reply To: Tolerances before or after anodizing?

Thanks for reaching out with a great question! Specifying a hard anodizing thickness of 15μ on your drawing is a solid start. Here’s the scoop: achieving exact thickness in anodizing can be a bit like...

View Article

Reply To: Tolerances before or after anodizing?

Hello there, so let me know if I understand correctly with this example. We consider making hard anodizing and indicate 15μ thickness on our drawing ; and determine our tolerance in accordance. Can we...

View Article

Reply To: Tolerances before or after anodizing?

Thank you, Pierre-Yves!

View Article


Reply To: Tolerances before or after anodizing?

Thank you!

View Article

Reply To: Tolerances before or after anodizing?

Hello Nick and AttilaAs a Production support engineer at Xometry, I could add that by default, when a drawing is submitted to us and an anodizing or other post-treatment is ordered, we consider that...

View Article

Reply To: Tolerances before or after anodizing?

Hello Nick, It’s great to hear from someone with a keen interest in the intricacies of CNC manufacturing, especially when it comes to the nuanced area of specifying tolerances about surface treatments...

View Article


Tolerances before or after anodizing?

Hey there, I have a question regarding the standard practice in the industry about specifying tolerances in relation to surface treatments like anodizing. Given the potential for anodizing to add a...

View Article

Browsing latest articles
Browse All 18 View Live